Name |
254SMO STUD BOLT |
Standard |
DIN975/DIN976,IFI136 |
Size Range |
M5-M64 or non-standard as requested |
Finish |
Bright&Clean |
Marking |
HT&FST or customization |
Material |
254SMO,UNS S31254,1.4547,F44 |
Grade |
Grade 70 |
Certificates |
EN10204-3.1B |
Non-standards |
OEM is available, according to drawing or samples |
Samples |
Samples available |
Package |
Bulk in box and then in cartons, then on pallets, or according to customers' requirement. |
Payment | T/T,Western Union |
Corrosion resistant alloy 254SMO similar grade
UNS |
AISI/ASTM |
ID | W.Nr |
S31254 | 254SMO | F44 | 1.4547 |
Chemical composition of corrosion-resistant alloy 254SMO
Alloy | % | Ni | Cr | Mo | Cu | N | C | Mn | Si | P | S |
254SMO | Min. |
17.5 | 19.5 | 6 | 0.5 | 0.18 | |||||
Max. | 18.5 | 20.5 | 6.5 | 1.0 | 0.22 | 0.02 | 1 | 0.8 | 0.03 | 0.01 |
Physical Properties of Corrosion Resistant Alloy 254SMO
Density |
8.0g/cm³ |
Melting point | 1320~1390℃ |
Minimum mechanical properties of corrosion-resistant alloy 254SMO at room temperature
Tensile strength Rm N/mm² |
Yield strength Rp0.2 N/mm² |
Elongation rate A5% |
650 | 300 | 35 |
Name |
254SMO STUD BOLT |
Standard |
DIN975/DIN976,IFI136 |
Size Range |
M5-M64 or non-standard as requested |
Finish |
Bright&Clean |
Marking |
HT&FST or customization |
Material |
254SMO,UNS S31254,1.4547,F44 |
Grade |
Grade 70 |
Certificates |
EN10204-3.1B |
Non-standards |
OEM is available, according to drawing or samples |
Samples |
Samples available |
Package |
Bulk in box and then in cartons, then on pallets, or according to customers' requirement. |
Payment | T/T,Western Union |
Corrosion resistant alloy 254SMO similar grade
UNS |
AISI/ASTM |
ID | W.Nr |
S31254 | 254SMO | F44 | 1.4547 |
Chemical composition of corrosion-resistant alloy 254SMO
Alloy | % | Ni | Cr | Mo | Cu | N | C | Mn | Si | P | S |
254SMO | Min. |
17.5 | 19.5 | 6 | 0.5 | 0.18 | |||||
Max. | 18.5 | 20.5 | 6.5 | 1.0 | 0.22 | 0.02 | 1 | 0.8 | 0.03 | 0.01 |
Physical Properties of Corrosion Resistant Alloy 254SMO
Density |
8.0g/cm³ |
Melting point | 1320~1390℃ |
Minimum mechanical properties of corrosion-resistant alloy 254SMO at room temperature
Tensile strength Rm N/mm² |
Yield strength Rp0.2 N/mm² |
Elongation rate A5% |
650 | 300 | 35 |